您的位置: 专家智库 > >

陈亮

作品数:4 被引量:10H指数:3
供职机构:大连理工大学更多>>
发文基金:国家自然科学基金中国航空科学基金中央高校基本科研业务费专项资金更多>>
相关领域:金属学及工艺一般工业技术更多>>

文献类型

  • 3篇期刊文章
  • 1篇会议论文

领域

  • 4篇金属学及工艺
  • 3篇一般工业技术

主题

  • 3篇TE
  • 3篇CU-MG
  • 2篇导电
  • 2篇导电率
  • 2篇
  • 2篇Y
  • 1篇铜合金
  • 1篇退火
  • 1篇维氏硬度
  • 1篇抗拉
  • 1篇抗拉强度
  • 1篇合金
  • 1篇合金性能
  • 1篇ROLLIN...
  • 1篇
  • 1篇ALLOY
  • 1篇ALLOYS
  • 1篇ANNEAL...
  • 1篇ALLOYI...
  • 1篇DEFORM...

机构

  • 4篇大连理工大学

作者

  • 4篇张兴国
  • 4篇陈亮
  • 4篇贾非
  • 3篇韩建宁
  • 3篇周秉文
  • 1篇亚斌
  • 1篇张美娟

传媒

  • 2篇Transa...
  • 1篇稀有金属材料...

年份

  • 2篇2014
  • 1篇2013
  • 1篇2010
4 条 记 录,以下是 1-4
排序方式:
Effects of alloying and deformation on microstructures and properties of Cu-Mg-Te-Y alloys被引量:5
2013年
New copper alloys with high mechanical properties and high electrical conductivity were prepared, and the effects of addition of minor Mg and Y elements on microstructures and properties were studied. The high tensile strength of above 510 MPa, high elongation of 11%and high electrical conductivity of over 63%IACS can be simultaneously obtained in Cu-0.47Mg-0.20Te-0.04Y alloy after deforming and annealing treatment. Effects of purification together with the grain refining by Y and solid-solution strengthening by Mg are appropriate for enhancing mechanical properties and electrical conductivity of the copper alloys.
陈亮周秉文韩建宁薛彦燕贾非张兴国
关键词:ALLOYINGDEFORMATION
镁和碲元素含量对导电铜合金性能影响的研究
研究了镁和碲元素含量对导电铜合金的显微组织、力学性能及导电率的影响。向铜中加入镁和碲元素进行合金的熔炼,并对其进行显微组织、抗拉强度和延伸率,以及导电性等性能的测试分析。结果表明,在铜中加入少量的镁元素和碲元素,与纯铜相...
张美娟陈亮亚斌贾非张兴国
关键词:铜合金抗拉强度导电率
文献传递
Effects of rolling and annealing on microstructures and properties of Cu-Mg-Te-Y alloy被引量:3
2014年
Microstructures and element distributions of the as-cast, hot-rolled and cold-rolled Cu-Mg-Te-Y alloys were studied. Effects of rolling process and annealing temperature on the properties of the Cu-Mg-Te-Y alloys were correspondingly investigated. The results indicate that the Mg element is homogeneously distributed in the matrix and the fragmentized Cu2Te phase is dispersed in the matrix after hot rolling. Then, the Cu2Te phase is further stretched to strip shape after the cold rolling process. The microstructures of the cold-rolled alloy keep unchanged for the sample annealed below 390 ℃ for 1 h. However, after annealing at 550 ℃ for 1 h, the copper alloy with fibrous microstructures formed during the cold rolling process recrystallizes, leading to an obvious drop of hardening effect and an increase of electrical conductivity. The Cu-Mg-Te-Y alloy with better comprehensive properties is obtained by annealing at 360-390 ℃.
陈亮韩建宁周秉文薛彦燕贾非张兴国
关键词:ROLLINGANNEALING
Cu-Mg-Te-Y合金退火工艺研究被引量:4
2014年
研究了退火温度和退火时间对冷轧变形后的Cu-Mg-Te-Y合金组织及性能的影响。结果表明:Cu-Mg-Te-Y合金在冷轧变形后,显微组织呈纤维状,内部晶粒取向改变,硬度提高,导电率降低;经过退火处理后,铜合金硬度下降,导电率回升,提高退火温度可明显提高合金伸长率;随退火时间延长,Mg原子从晶格中脱出,通过位错等扩散通道,在Cu2Te相周围偏聚,使导电率提高,但再结晶新晶粒的出现,晶界增多,使导电率降低,综合作用使合金的导电率明显提高;退火温度在360~390℃,退火时间1 h以内时,Cu-Mg-Te-Y合金可以得到最佳的综合性能。
韩建宁陈亮周秉文薛彦燕贾非张兴国
关键词:退火导电率维氏硬度